K-Plate
Tin plate with superior corrosion resistance to mild acid food
products; must meet four (4) special property tests : 1. Pickle lags 10 or less. 2. Tin
crystal size ASTM 9 or larger. 3. ISV (iron solution value) 20 micro grams Fe or less. 4.
ATC (Alloy tin couple - American Can test) or AMP (Aerated Media Polarization test) Avg.
0.050 micro amps/sq. cm. Or less 95% 0.085 or less. No test over 0.120.